Chemical Composition

Grade Symbol UNS Number Alloy Elements Composition %
F91 K90901 9% chromium, 1% molybdenum, 0.2% vanadium plus columbium and nitrogen Carbon 0.08 - 0.12
Manganese 0.30 - 0.60
Phosphorus 0.020 max
Sulfur 0.010 max
Silicon 0.20 - 0.50
Nickel 0.40 max
Chromium 8.0 - 9.5
Molybdenum 0.85 - 1.05
Columbium 0.06 - 0.10
Nitrogen 0.03 - 0.07
Aluminium 0.02 max
Vanadium 0.18 - 0.25
Titanium 0.01 max
Zirconium 0.01 max

Mechanical Properties

PropertyValue
Tensile Strength, min, ksi [MPa] 90 [620]
Yield Strength, min, ksi [MPa] 60 [415]
Elongation in 2 in. [50mm] or 4D, min, % 20
Reduction or Area, min, % 40
Brinell Hardness Number, HBW 190-248

Heat Treatment

After hot working, forgings shall be cooled to a temperature below 1000 °F [538 °C] prior to heat treating in accordance with the requirements.