Chemical Composition

Grade Symbol UNS Number Alloy Elements Composition %
F6NM S41500 13% chromium,
4% nickel
Carbon 0.05 max
Manganese 0.50 - 1.00
Phosphorus 0.030 max
Sulfur 0.030 max
Silicon 0.60 max
Nickel 3.5 - 5.5
Chromium 11.5 - 14.0
Molybdenum 0.50 - 1.00

Mechanical Properties

PropertyValue
Tensile Strength, min, ksi [MPa] 115 [790]
Yield Strength, min, ksi [MPa] 90 [620]
Elongation in 2 in. [50mm] or 4D, min, % 15
Reduction or Area, min, % 45
Brinell Hardness Number, HBW 295 max

Heat Treatment

After hot working, forgings shall be cooled to a temperature below 1000 °F [538 °C] prior to heat treating in accordance with the requirements.