Chemical Composition

Grade Symbol Alloy Elements Composition %
F5 4% to 6% Chromium Carbon 0.15 max
Manganese 0.30 - 0.60
Phosphorus 0.030 max
Sulfur 0.030 max
Silicon 0.50 max
Nickel 0.50 max
Chromium 4.0 - 6.0
Molybdenum 0.44 - 0.65

Mechanical Properties

PropertyValue
Tensile Strength, min, ksi [MPa] 70 [485]
Yield Strength, min, ksi [MPa] 40 [275]
Elongation in 2 in. [50mm] or 4D, min, % 20
Reduction or Area, min, % 35
Brinell Hardness Number, HBW 143-217

Heat Treatment

After hot working, forgings shall be cooled to a temperature below 1000 °F [538 °C] prior to heat treating in accordance with the requirements.