Chemical Composition

Grade Symbol UNS Number Alloy Elements Composition %
F316LN S31653 18 chromium, 8 nickel,
modified with molybdenum
and nitrogen 316LNG
Carbon 0.030 max
Manganese 2.00 max
Phosphorus 0.045 max
Sulfur 0.030 max
Silicon 1.00 max
Nickel 11.0–14.0
Chromium 16.0 - 18.0
Molybdenum 2.00 - 3.00
Nitrogen 0.10 - 0.16

Mechanical Properties

PropertyValue
Tensile Strength, min, ksi [MPa] 75 [515]C
Yield Strength, min, ksi [MPa] 30 [205]
Elongation in 2 in. [50mm] or 4D, min, % 30
Reduction or Area, min, % 50

Heat Treatment

After hot working, forgings shall be cooled to a temperature below 1000 °F [538 °C] prior to heat treating in accordance with the requirements.