Chemical Composition
Grade Symbol |
UNS Number |
Alloy |
Elements |
Composition % |
F316H |
S31609 |
18 chromium, 8 nickel, modified with molybdenum 316HG |
Carbon |
0.04 - 0.10 |
Manganese |
2.00 max |
Phosphorus |
0.045 max |
Sulfur |
0.030 max |
Silicon |
1.00 max |
Nickel |
10.0 - 14.0 |
Chromium |
16.0 - 18.0 |
Molybdenum |
2.00 - 3.00 |
Mechanical Properties
Property | Value |
Tensile Strength, min, ksi [MPa] |
75 [515] |
Yield Strength, min, ksi [MPa] |
30 [205] |
Elongation in 2 in. [50mm] or 4D, min, % |
30 |
Reduction or Area, min, % |
50 |
Heat Treatment