Chemical Composition

Grade Symbol UNS Number Alloy Elements Composition %
F304 S30400 18 chromium,
8 nickel 304G
Carbon 0.08 max
Manganese 2.00 max
Phosphorus 0.045 max
Sulfur 0.030 max
Silicon 1.00 max
Nickel 8.0 - 11.0
Chromium 18.0 - 20.0
Nitrogen 0.10

Mechanical Properties

PropertyValue
Tensile Strength, min, ksi [MPa] 75 [515]
Yield Strength, min, ksi [MPa] 30 [205]
Elongation in 2 in. [50mm] or 4D, min, % 30
Reduction or Area, min, % 50
Brinell Hardness Number, HBW --

Heat Treatment

After hot working, forgings shall be cooled to a temperature below 1000 °F [538 °C] prior to heat treating in accordance with the requirements.